# 48, Noothanchery, Madambakkam, Chennai - 600 126, India. Ph: +91 44 22781148 Fax: +91 44 22781362 Email: info@tianode.com | tianode@gmail.com
MMO / PLATINIZED ICCP ANODES
Impressed Current Cathodic Protection (ICCP) is an economical method for controlling corrosion on above ground storage tank bottoms, buried and submerged structures, deep and conventional ground beds fresh, brackish and salt water electrolytes, offshore platforms, condensers, water tanks and pressure vessels. Ti Anode Fabricators Pvt Ltd, Chennai is manufacturing the following anodes for ICCP (Impressed Current Cathodic Protection) application.
Range of our Impressed Current Cathodic Protection - ICCP Anodes
Material of Construction
  1. Substrate
  2.  
    Titanium
          Wire & Rod		: ASTM B 348 Gr. 1 or 2
          Tube			: ASTM B 337 / 338 Gr. 1 or 2
          Mesh, Ribbon, Strip & Disc	: ASTM B 265 Gr. 1
    Niobium
          Wire & Rod		: ASTM B 392 Gr. R04210
          Tube			: ASTM B 337 / 394 Gr. R04210
          Mesh, Ribbon, Strip & Disc	: ASTM R04210
    
  3. Catalyst

  4. Ir, Ta, Pt, Ru, Pd, Ti & others, depends on application.

  5. Cables

  6. EPR/CSPE, EPR/GSWB/CSP, HMWPE, XLPE/PVC, SWA/PVC, PVDF

  7. Coke Breeze
  8.  
    Size		: 1.0mm;
    Fixed carbon	: 98.0%;
    Ash		: 1.0%;
    Moisture		: 0.5%;
    Volatile matter	: 0.5%;
Design & Application Specification of MMO Coated Titanium Anodes
Electrolyte Maximum Current Density Maximum Current Density Anode Life
Carbonaceous Backfill 50 A/m2 20 years
Calcined Petroleum Coke 100 A/m2 20 years
Fresh Water 100 A/m2 20 years
Brackish Water 300 A/m2 20 years
Sea Water 600 A/m2 20 years
Design & application specification of Platinised Titanium / Niobium Anode
Substrate Titanium Niobium Tantalum
Max. Allowable operating voltage 12V 40V 80V
Wire length 100m 50m 50m
Wire diameter 1 / 2 / 3 / 4 mm
Tube length Max. 3000 mm
Tube diameter 12 / 16 / 19 / 25 mm
Rod length Max. 3000 mm
Rod diameter 6 / 8 / 10 /12 / 16 / 20 / 25 mm
Mesh length Max. 2500 mm
Mesh width Max. 800 mm
Pt - coating thickness 5 / 7.5 / 10 µm
Consumption rate Approx. 8 to 16mg / A year In sea water

Description PTA PNA MMOA
PH Level: (range) 1.0-12.0 1.0-10.0 1.0-12.0
Platinum / mixed oxide layer tk. 1.5-20.0 1.5-15.0 8.0
Fluorides content (max) 50mg/l 500mg/l 50mg/l
Allowable current (max) 50A/dm2 100A/dm2 50A/dm2



Cathodic Protection Anodes
CPCC Titanium Tubular Anodes for Cathodic Protectin


Titanium Embbeded Civil Probe Anode for Cathodic Protectin
Titanium Electrolyzers


Titanium Anode Baskets
Titanium Conductor Bars for Impressed Current Cathodic Protection


Platinised Titanium Anodes
Titanium Rod Anodes for Impressed Current Cathodic Protection


Platinum & MMO Coated Anodes
Titanium Disc and Strip Anodes for ship


Platinum & MMO Coated Anodes
MMO Coated Titanium Ribbon / Wire Anodes

Please visit for...
CP Anodes
PT Anodes
Electrolyzers
Chlorinators
Ti Projects
TitanicTrade
Alibaba TrustPass

 Send Enquiry
 Printable Version
Home | Profile| Technologies| Products| Application| Certification| Raw Material| Water Car
Selection Guide | CP Anode| PT   Anode| Electrolyzers| Chlorinators| Ti Projects| Route Map| Contacts